Sign In | Join Free | My fazendomedia.com |
|
Brand Name : Rongsheng
Model Number : Magnesia Brick
Certification : ISO9001
Place of Origin : Henan, China
MOQ : 1 TON
Payment Terms : L/C, T/T, Western Union
Supply Ability : 6000 Ton/Tons per Month Free samples refractories fire mgo bricks for sale
Delivery Time : 20-30DAYS
Packaging Details : 1.On wooden pallets with plastic cover 2.According to customer's demands for High quality magnesia brick 92% 95% 97%98% mgo fired magnesia refractories brick for kiln fire-resistant
Shape : Brick
Material : burned magnesia or electric fused
SiO2 Content (%) : customizable
Al2O3 Content (%) : customizable
MgO Content (%) : customizable
CrO Content (%) : customizable
SiC Content (%) : customizable
Refractoriness : Super-Class (Refractoriness> 2000
Applications : Iron steel furnace,glass furnace,cement kiln
Feature : High refractoriness
Keyword : Free samples refractories fire mgo bricks for sale
High Quality Magnesia Brick 92% 95% 97%98% Mgo Fired Magnesia Refractories Brick For Kiln Fire-Resistant
Product information
Magnesite brick using density sintered magnesia as raw material, it has high refractoriness,resistance to erosion ability, load soft higher characteristic, suitable for titanium slagfurnace molten pool and furnace wall slag line work layer.
Feature
1. High refractoriness,usually the refractoriness is above 2000°C.
2. Refractoriness under load about 1500-1550°C because of poor high-temperature intensity.
3. Strong ability to resist basic (alkaline) slag,can not contact with acid refractory material.
4. Poor Thermal shock resistance,so keep the temperature of furnace stabilized.
5. Poor Volume stability at high temperature,must set aside appropriate expansion joint when laying brick.
6. Strong ability of thermal conductivity,sometime need insulating material.
Physical and chemical indexes
Item | MZ-97 | MZ-95 | MZ-93 | MZ-91 |
MgO % | ≥97 | ≥95 | ≥93 | ≥91 |
SiO2 % | ≤1.0 | ≤2.0 | ≤3.5 | - |
CaO % | - | ≤2.0 | ≤2.0 | ≤3.0 |
Apparent porosity/% | ≤16 | ≤16 | ≤18 | ≤18 |
Cold crushing strength/ Mpa | ≥60 | ≥60 | ≥60 | ≥60 |
Refractoriness under load, 0.2MPa, °C | ≥1700 | ≥1650 | ≥1620 | ≥1560 |
Reheating Linear Change(1650 °C,2h) /% | 0~-0.2 | 0~-0.3 | 0~-0.4 | 0~-0.4 |
Shapes &Sizes
Straight | Split | Arch | Wedge | Tile | Other Shape |
L×W×H(mm) 230×114×65 230×114×75 |
L×W×H (mm) 230×114×25 230×114×32 230×114×37 230×114×50 |
L×W×H/h(mm) 230×114×65/45 230×114×65/55 230×114×75/45 230×114×75/55 230×114×75/65 |
L×W×H/h (mm) 230×114×65/45 230×114×65/55 220×114×75/45 220×114×75/55 220×114×75/65 |
L×W×H (mm) 230×230×38 230×230×50 230×230×65 230×230×75 |
Key brick, Skew brick, Soap, Checker, Neck, Taper, |
Applications
1. Iron Steel Industry
steelmaking furnace lining, ferroalloy furnace, metal mixer furnace lining, converter lining, arc furnace wall and furnace bottom, soaking furnace, heating furnace bottom
2. Non-ferrous metallurgical industry
copper,nickel,lead,zinc,tin smelting furnace lining, refined copper reverberatory furnace,ore electric furnace lining
3. Glass Industry
glass furnace regenerator checker
4. Building Material Industry
lime kiln,cement kiln
5. Refractory Material Industry
High temperature calcination kiln,shaft kiln and tunnel kiln
![]() |
92% 95% 97% 98% MgO Refractory Magnesia Bricks Images |